Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® B3WG12 HSP BK23228 - PA6-GF60 - BASF

Material Data Center offers the following functions for Ultramid® B3WG12 HSP BK23228:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid B datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Glass fibre reinforced and heat ageing resistant injection moulding grade with high flowability and excellent surface quality for structural parts with very high stiffness requirements.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 22 / * cm³/10min ISO 1133
Temperature 275 / * °C -
Load 5 / * kg -
Molding shrinkage, parallel 0.3 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.6 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 21500 / 14000 MPa ISO 527
Stress at break 250 / 170 MPa ISO 527
Strain at break 2.5 / 4 % ISO 527
Charpy impact strength, +23°C 95 / 100 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 90 / 90 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 16 / 20 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 16 / 16 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 220 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 210 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 16 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 87 / * E-6/K ISO 11359-1/-2
Other propertiesdry / condUnitTest Standard
Water absorption 4 / * % Sim. to ISO 62
Humidity absorption 1 / * % Sim. to ISO 62
Density 1720 / - kg/m³ ISO 1183
Bulk density 700 kg/m³ -
Material specific propertiesdry / condUnitTest Standard
ISO Data
Viscosity number 105 / * cm³/g ISO 307, 1157, 1628
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 300 °C ISO 294
Injection Molding, mold temperature 100 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 4 h -
Processing humidity ≤0.15 % -
Melt temperature 280 - 310 °C -
Mold temperature 90 - 120 °C -
Diagrams
Viscosity-shear rate , Ultramid® B3WG12 HSP BK23228, PA6-GF60, BASF
Shearstress-shear rate , Ultramid® B3WG12 HSP BK23228, PA6-GF60, BASF
Dynamic Shear modulus-temperature , Ultramid® B3WG12 HSP BK23228 (dry), PA6-GF60, BASF
Dynamic Shear modulus-temperature , Ultramid® B3WG12 HSP BK23228 (cond.), PA6-GF60, BASF
Stress-strain , Ultramid® B3WG12 HSP BK23228 (dry), PA6-GF60, BASF
Stress-strain , Ultramid® B3WG12 HSP BK23228 (cond.), PA6-GF60, BASF
Secant modulus-strain , Ultramid® B3WG12 HSP BK23228 (dry), PA6-GF60, BASF
Secant modulus-strain , Ultramid® B3WG12 HSP BK23228 (cond.), PA6-GF60, BASF
Tensile modulus-temperature , Ultramid® B3WG12 HSP BK23228 (dry), PA6-GF60, BASF
Tensile modulus-temperature , Ultramid® B3WG12 HSP BK23228 (cond.), PA6-GF60, BASF
Characteristics
Processing
Injection Molding
Delivery form
Pellets, Black
Additives
Lubricants, Release agent
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
North America, Europe
Other text information
Injection molding
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 280 - 310 °C
injection molding, Melt temperature, recommended: 290 °C
injection molding, Mold temperature, range: 90 - 120 °C
injection molding, Mold temperature, recommended: 100 °C
injection molding, Dwell time, thermoplastics: 10 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.